New catalytic FeCrAlloy premixed fiber burners for natural gas combustion in domestic applications were developed according to an accurate microstructural design consisting of subsequent optimized steps: (i) optimal preoxidation of the FeCrAlloy fiber mat so as to develop the best possible Al2O3 layer for simultaneous prevention of deeper fiber oxidation at high temperature and optimal catalyst anchoring over the fiber surface, (ii) deposition via the either spray-pyrolysis or wash-coating technique of a previously developed perovskite catalyst (LaMnO3â 17MgO), and (iii) extensive testing of the catalyst-burner bonding strength and burner performance. Even after extensive aging under practical operating conditions (repeated on-off cycles and prolonged durations under high-temperature radiating conditions), the best developed burners (i.e., those obtained by spray pyrolysis) exhibit very limited catalyst loss and still remarkably lower (30-50%) NO and CO emissions than noncatalytic, virgin FeCrAlloy burners at the specific power densities of practical interest (150-650 kW/m2).

Optimal microstructural design of a catalytic premixed FeCrAlloy fiber burner for methane combustion / Ugues, Daniele; Specchia, Stefania; Saracco, Guido. - In: INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH. - ISSN 0888-5885. - 43:9(2004), pp. 1990-1998. [10.1021/ie034202q]

Optimal microstructural design of a catalytic premixed FeCrAlloy fiber burner for methane combustion

UGUES, Daniele;SPECCHIA, STEFANIA;SARACCO, GUIDO
2004

Abstract

New catalytic FeCrAlloy premixed fiber burners for natural gas combustion in domestic applications were developed according to an accurate microstructural design consisting of subsequent optimized steps: (i) optimal preoxidation of the FeCrAlloy fiber mat so as to develop the best possible Al2O3 layer for simultaneous prevention of deeper fiber oxidation at high temperature and optimal catalyst anchoring over the fiber surface, (ii) deposition via the either spray-pyrolysis or wash-coating technique of a previously developed perovskite catalyst (LaMnO3â 17MgO), and (iii) extensive testing of the catalyst-burner bonding strength and burner performance. Even after extensive aging under practical operating conditions (repeated on-off cycles and prolonged durations under high-temperature radiating conditions), the best developed burners (i.e., those obtained by spray pyrolysis) exhibit very limited catalyst loss and still remarkably lower (30-50%) NO and CO emissions than noncatalytic, virgin FeCrAlloy burners at the specific power densities of practical interest (150-650 kW/m2).
File in questo prodotto:
Non ci sono file associati a questo prodotto.
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11583/1405885
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo