The dies employed for the hot extrusion of aluminium alloys are subjected to repeated cycles of nitriding, or nitrocarburising, after service periods of given length. Three dies, fabricated with ISO X40CrMoV5-1 (AISI H13) steel and liquid nitrocarburised, were examined either in the asfabricated condition, or after one service period, or after 12 nitrocarburising and service cycles (end of life). Samples cut from the die subjected to one service period were re-nitrocarburised for increasing durations and similarly examined. The examination methods included X-ray diffraction, metallography, microhardness profile measurements and SEM fractography. The service temperature induced microstructural modifications in the core and in the case. Microcracks and wear craters, due to adhesive wear, occurred at the bearing surfaces. The wear mechanisms at a bearing surface, the microstructural evolution close to the same surface, the fatigue crack nucleation and early growth, and their interrelations and consequences during the whole die life are discussed.

Damage of repeatedly nitrocarburised steel dies for aluminium extrusion / Matteis, Paolo; Scavino, Giorgio; Quadrini, E.; Perucci, P.; Firrao, Donato. - In: SURFACE ENGINEERING. - ISSN 0267-0844. - STAMPA. - 25:7(2009), pp. 507-516. [10.1179/026708408X339073]

Damage of repeatedly nitrocarburised steel dies for aluminium extrusion

MATTEIS, PAOLO;SCAVINO, Giorgio;FIRRAO, Donato
2009

Abstract

The dies employed for the hot extrusion of aluminium alloys are subjected to repeated cycles of nitriding, or nitrocarburising, after service periods of given length. Three dies, fabricated with ISO X40CrMoV5-1 (AISI H13) steel and liquid nitrocarburised, were examined either in the asfabricated condition, or after one service period, or after 12 nitrocarburising and service cycles (end of life). Samples cut from the die subjected to one service period were re-nitrocarburised for increasing durations and similarly examined. The examination methods included X-ray diffraction, metallography, microhardness profile measurements and SEM fractography. The service temperature induced microstructural modifications in the core and in the case. Microcracks and wear craters, due to adhesive wear, occurred at the bearing surfaces. The wear mechanisms at a bearing surface, the microstructural evolution close to the same surface, the fatigue crack nucleation and early growth, and their interrelations and consequences during the whole die life are discussed.
File in questo prodotto:
File Dimensione Formato  
2303431.pdf

accesso aperto

Tipologia: 2. Post-print / Author's Accepted Manuscript
Licenza: PUBBLICO - Tutti i diritti riservati
Dimensione 1.58 MB
Formato Adobe PDF
1.58 MB Adobe PDF Visualizza/Apri
Pubblicazioni consigliate

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11583/2303431
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo